1. The pre-processed fabric must be refined and clean. The residual surfactant will affect the waterproof effect. The pH of the fabric before finishing must not be alkaline;
2. Choose the appropriate baking temperature and time. Too high temperature and long time will reduce the waterproof effect;
3. When it is necessary to improve the penetration effect during padding, 2-5g/l isopropyl alcohol or 0.2-0.5g/l non-silicon foam inhibitor penetrant can be added;
4. Softener may have a great impact on the waterproofing effect. If you want to use it in the same bath, you must test it first;
5. Subsequent processing such as calendering, scratching, and coating may have a great impact on the waterproofing effect, and it is necessary to test and adjust the process in advance;
6. There may be problems with color change and color fastness during processing, and pre-testing is required.
Our company produces and sells (C4, C6, fluorine-free, highly concentrated, etc.)
Extended reading: https://www.yingjietex.com/product/NYLON-SATIN -COATED-Fabric.html
Extended reading: https://www.alltextile. cn/product/product-3-610.html
Extended reading: https://www.yingjietex.com/product/Full-dull-NyLon-Ripstop-Fabric.html
Extended reading:https://www.tpu-ptfe.com/post/3275.html
Extended reading: https://www.yingjietex.com/product/DE-17-Memory-Fabric.htm